Metallurgical chromite ore grade and mining technical indicators

By "chrome iron ore grade and mining technology indicators" can be clearly chromite mining cutoff grade and industrial grade guidance for chromite ore miners were estimated value.

Metallurgical grade chromite ore and mining with technical indicators

project Deposit and ore type
Endogenous deposit
Rich mine Lean mine
ω(Cr2O3) Boundary grade ≥25 ≥5~8
The lowest industrial grade ≥32 ≥12
The lowest available thickness m 0.3~0.5 1.0
Stone removal thickness m 0.5 1.0

Note 1: chrome ore or concentrate for metallurgy, ω(Cr2O3)/ω(FeO)>2 during pyrometallurgical smelting (metal chromium is not restricted by wet method); ω(SiO2)≤8% The ore-heating method is not limited by the smelting of high-carbon ferrochrome; ω(P)≤0.07%, ω(S)≤0.05%.

2: chrome ore or concentrate for refractory materials, ω (SiO2) ≤ 10%, ω (CaO) ≤ 3%, ω (FeO) ≤ 14%.

3: chrome ore or concentrate for chemical industry ω (SiO2) ≤ 8%, ω (A12O3) ≤ 15%.

4: chrome ore for diabase cast stone, ω (Cr2O3) ≥ (10% ~ 20%), ω (SiO2) < 10%.

5: When the total amount is selected from PGE for an associated chromite reaches 10-6 (0.3 ~ 0.4) ×, evaluation should be made.

6: The selection of lean grades is generally twice the grade of tailings.

7: The selection of the minimum mining thickness of the rich ore is 0.5m for the single ore layer and 0.3m for each layer of the complex ore layer.